HN-E10 Electrolytic Degreasing Powder
Commodity Name
HN-E10 Electrolytic Degreasing Powder
Composition and Working Conditions
For steel parts:
HN -E10 40~80g/L
Temperature 30~70℃
Time 0.5~5 minutes
Current density 3~8A/dm2
For copper and coppery alloy parts:
HN -E10 40~60g/L
Temperature 25~40℃
Time 20~60 seconds
Current density 1~3A/dm2
Application and Advantage
1. Suitable for different kinds of electrolytic degreasing on carbon steel, alloy steel and copper alloy parts, etc.
2. It has excellent degreasing/ emulsifying ability. Components wont be second-polluted after taking out
from tank.