HN-3000 Aluminum Alloy Zincate Process
Commodity Name
HN-3000 Aluminum Alloy Zincate Process
Composition and Working Conditions

 

HN-3000                    550~600mL/L

Temperature             16~30℃

Time                          20~120s

 

Application and Advantage

 

1. Alloy of zinc, copper, iron and nickel.

2. Good adhesion can be got even in low aluminum alloy.

3. After zinc plating, electroless nickel or plating nickel can be done directly.

4. HN-3000C and HN-3000B, or just HN-3000, can be used to supplement the concentration of metal and 

alkali, which makes the solution stable and easy to control. 

5. Especially suitable for aluminum alloy wheel plating.